Internal quality control criterion for zirconia-corundum refractory bricks
Item Indicator
AZS33-Y AZS36-Y AZS41-Y
Chemical content/% AL2O3 Allowance
ZrO2 32.00-36.00 35.00-40.00 40.00-44.00
SiO2 W 16.00 14.00 13.00
N&O W 1.45 1.45 1.30
(FezO'+TiOz+CaO+MgO+NazO+KzO) W 2.00 2.00 2.00
(Fe2O3+TiO2) W 0.30 0.30 0.30
Bulk density / (g/cm3) 3.75 3.80 3.95
Apparent porosity/% W 1.5 1.00 1.00
Resistance to glass melt rate under static state (ordinary soda-lime glass, 
1500° CX36h)/(mm/24h) W
1.60 1.50 1.30
Initial segregation temperature at glass phase/° C N 1400 1400 1400
Bubble rate (ordinary soda-lime glass, 1300° CX10h)/% W 2.00 1.5 1.00
Glass phase seepage (1500° CX4h)/% W 2.00 3.00 3.00
Thermal expansion coefficient (room temperature -1000℃)/% W Provide measured data
Volume 
7kg/m3
PT 、 QX 〉 3400 3450 3550
ZWS 〉 3600 3700 3850
WS 〉 3700 3750 3900
a For products with unit weight over 50kg
Appearance
 (Crack)
Map cracking Allowable
Width W1.0 Cracks longer than 1/2 of the face width not allowed
Width between 1.0 -2.0 Cracks longer than 30mm not allowed
Crossing-edge cracks Cracks crossing one edge allowed, crack in length greater than 1/5 of the face width not allowed
Surface attachments or other fused materials Not allowed
Squareness requirements for products with side length < 500mm shall be determined by the supplier and the buyer through negotiation